Assignment
Process pieces of epoxy composite into a fraction of 0-100 microns (0-0.100 mm) and prepare samples from this fraction for further testing.
Process and Outcome
First, the incoming material had to be crushed to the optimum fraction for micronisation, with a particle size ≤ 5 mm. This material was then micronised to the fraction required by the customer and the samples were prepared.
Input material (left) and final product (right)